1. Why Bed Adhesion Problems Happen with ABS
ABS filament has a high melting temperature (around 220-250°C), and it tends to shrink as it cools, leading to warping and lifting off the print bed. The bed adhesion issues primarily arise because the first layer cannot grip the bed surface properly, causing corners to lift or prints to fail entirely.

2. Key Factors Influencing ABS Bed Adhesion
Temperature
ABS requires a hotbed temperature between 90-110°C to maintain a warm surface for proper adhesion. Insufficient bed temperature is one of the most common reasons ABS doesn’t stick. In addition, a stable ambient temperature is needed to prevent the print from cooling too fast, which can lead to warping.
Bed Surface
The choice of print bed surface can greatly affect adhesion. Some surfaces, like PEI sheets, offer excellent grip, while others, like glass, may need additional adhesive materials. Experimenting with bed surfaces is key to determining what works best for ABS.

Print Settings
Your printer settings can influence adhesion:
- First Layer Height: A thicker first layer can provide better contact with the bed.
- Speed and Flow Rate: Printing the first layer slower and with a higher flow rate allows the material to settle and stick better.
3. Tools and Materials to Improve ABS Bed Adhesion
Bed Adhesives
- Glue Stick: A simple solution that works well with ABS, providing a consistent adhesive layer.
- ABS Slurry: A homemade adhesive made by dissolving ABS in acetone, which can create a strong bond on the bed.
- Hairspray: Certain hairsprays (usually the unscented ones) are great for providing an extra tacky layer.

Specialized Print Beds
- PEI (Polyetherimide) Sheets: These are often recommended for ABS due to their high-temperature resistance and stickiness.
- Glass Beds: While common, glass needs additional adhesive (glue or slurry) to properly hold ABS.
- BuildTak or Magnetic Sheets: These specialized surfaces are designed to improve adhesion for all types of filaments, including ABS.

4. Step-by-Step Fixes for ABS Bed Adhesion Problems
Proper Bed Leveling
Even slight bed misalignments can cause adhesion issues. A properly leveled bed ensures that the first layer is consistently in contact with the surface. Use a feeler gauge or a piece of paper to manually adjust the bed if necessary.

Using an Enclosure for ABS Printing
Enclosures help maintain a stable temperature around the printer, minimizing warping. Commercial enclosures are available, but many users create DIY enclosures using materials like acrylic sheets or cardboard boxes.

Optimizing First Layer Settings
- Increase Bed Temperature: Ensure your bed is heated to 90-110°C.
- Reduce Speed for First Layer: Lower the print speed to 20-30mm/s to allow better adhesion.
- First Layer Height: Increasing the height to 0.2-0.3mm helps improve grip.
5. Common Case Studies and Solutions
Case 1: Warping at the Corners
Problem: The corners of your ABS print lift off the bed during printing.
Solution: Ensure bed leveling, apply an ABS slurry, and use brims to anchor the print edges to the bed. Enclosures can also prevent drafts that lead to cooling and warping.

Case 2: First Layer Not Sticking at All
Problem: The first layer of ABS refuses to adhere to the bed.
Solution: Check your bed temperature, level the bed, and apply a glue stick or ABS slurry. Ensure your nozzle distance is properly calibrated.

6. Advanced Techniques for Improving Adhesion
Brims, Rafts, and Other Adhesion Helpers
Brims extend outward from the print and increase surface area, making it easier for the object to stay stuck. Rafts provide a thick base for the print, which can help with difficult adhesion problems.

Post-Processing: Sanding and Cleaning the Bed
Before every print, it’s essential to clean the bed with isopropyl alcohol. A lightly sanded glass surface can improve adhesion, but be cautious not to damage the bed material.
7. Summary of Best Practices
- Maintain a stable temperature (hotbed and ambient).
- Use proper bed adhesives like glue sticks or ABS slurry.
- Level the bed accurately and use an enclosure when possible.
- Optimize your print settings for the first layer, including speed, height, and extrusion rate.
8. Conclusion
Achieving good bed adhesion with ABS can be challenging, but with the right techniques, tools, and knowledge, you can solve most adhesion issues. By properly preparing the bed, optimizing printer settings, and using adhesive solutions like glue sticks or ABS slurry, your prints can adhere better, reducing warping and improving overall print quality.